Cobalt Molybdenum Catalyst Product Description characteristics: the catalyst which has the advantage of high HDS, good compression resistance and abrasive resistance , low loading density , high space velocity and renewable use, takes modified alumina as carrier, with molybdenum and cobalt as the active components. ApplicationIt is mainly used for prehydrogenation of high sulphur reforming material and kerosene hydrogenation to produce aviation kerosene. Physical-chemical properties:
Shape | Trilobal extrudate |
Diameter mm | 1.2-1.8 |
Crushing strength | >120N/CM |
CoO:wt | 3.0-4.0 |
MoO:wt | 18-22 |
Bulk density kg/l | 0.76-0.86 |
Surface area:m2/g | 220-280 |
Pore volume:ml/g | 0.4-0.5 |
Activity index:
Process parameters | Hydrogen partial pressure,Mpa | temperature | Space velocity hr-1 | Hydrogen to oil ratio,V/V |
1.6 | 270 | 8.0 | 80 |
Raw oil | Iranian atmosphere distillation gasoline |
Product oil | sulfur max 0.5ppm,Nitrogen max0.5ppm |
Contact us if you need more details on Molybdenum Catalyst. We are ready to answer your questions on packaging, logistics, certification or any other aspects about Cobalt Acetate Catalyst、Molybdenum Catalyst. If these products fail to match your need, please contact us and we would like to provide relevant information.
Product Categories : Custom Fabrication Services > Molybdenum Product